CEM IV / B (P) 32.5 R

The cement is produced by grinding at least one type of mineral additive (pozzolana) prescribed by standards (max. %55) with portland clinker by addition of a certain amount of retarder (generally gypsum).

The product delivers the strength values respectively in late periods compared to CEM I and CEM II types. Water/cement ratio is respectively higher. It is much more resistant to alkali and aggregate reactions. It is best for repairing works, foundation filling and used in stucco and building chemicals manufacturing.

Packing Type: Sold in bulk or in 50 kg. kraft bags. Big-bags or sling bags.

Quality Control: Our product is certified to use CE marking in Europe.

Physical PropertiesKÇSStandartUnit
Initial Setting Time230Min. 75Minute
Final Setting Time295Minute
Specific Gravity1Maks. 10mm
Specific Surface (Blaine)4650cm²/g
Liter Weight845g/1
2 Days Strength18Min. 10MPa
28 Days Strength38Min. 32,5
Max. 52,5
MPa

 

 
Chemical PropertiesKÇSStandartUnit
SO³2.45Max. 3.5%
C1-0.0129Max. 0.1%
Puzzuolana TestPosittiveStatisfies The Test